December 18, 2007 – 8:04 pm
Construction Injection Anchor|Marble Mastice
 |
Main composition
· Polyurethane modified propenoicester
·Peroxide
·Quartz powder
Application
·Construction joint of concrete iron,structural fixing of broadening of expressway,reinforcement of bridges,reservoir,restoration of old buildings. |
| |
Main properties
·Two composition formulation
·Free of styrene
·Water resistant,acid and alkaline resistant,freeze resistant,
 not sensitive to humidity.
·Ageing resistant,fire—proofing and thermal isolation carl be used
·The pre-laid steel parts.
Packing specification
360ml/item 24items/ctn
Safety rule
·Discard the colloid injecte dout at the begining till,tevisible
 uniform color being seen.
·Continuous operation recommended in case of waste.
·Do not apply on the wetting platform.
·Make sure the aperture is cleaned thoroughly.
·Workable temperature ranges from -10℃ to 40℃.
·Recommended dosage is 2/3 the volume of aperture to full.
·Inject the colloid from the bottom of the aperture.
·12 months if stored in cool places avoiding lightening.
 Clean with acetone after application.
·Refer to the application directions on the package. |
web link:www.dalishi.com.cn
Tags: Binder, Construction Injection Anchor, Marble Mastice